A Kevlar fiber was annealed at 400 °C under the condition of constant length, and then fibrillar fragments were obtained by tearing them off from the fiber.The fragments thus prepared were used as specimens for TEM. Figure 1.10(a) is the dark-field image of the specimen using the 006 meridional reflection, showing a periodic banded texture which consists of alternating bright …